Long-Term Study Reveals How Humidity Affects the Durability of Biodegradable Thermoplastic Polymers

  • Researchers at IMDEA Materials identify hexagonal boron nitride as a promising additive for improving the long-term stability of biodegradable PLA under humid conditions

As the demand for sustainable alternatives to conventional plastics continues to grow, biodegradable polymers such as poly(lactic acid) (PLA) are attracting increasing attention for applications ranging from packaging to consumer products.

However, the long-term durability of these materials under humid conditions remains a critical challenge.

In a new study published in Polymer Degradation and Stability, researchers from IMDEA Materials Institute have investigated how prolonged exposure to heat and humidity affects the performance of PLA reinforced with different two-dimensional (2D) nanomaterials.

The work provides valuable insights into the mechanisms responsible for material degradation and highlights effective strategies for extending the service life of bio-based polymers.

The researchers behind the publication include Petronela Chovancová, Miguel Hernández del Valle, Dr. Maciej Haranczyk and Dr. Juan Pedro Fernández Blázquez.

While PLA is one of the most widely used biodegradable polymers, its susceptibility to moisture-induced degradation can limit its use in applications requiring long-term reliability.

“Previous studies have often focused on short-term water immersion tests, but these conditions do not always accurately reflect the variety of environments materials experience during storage or service,” explained Chovanvocá.

To address this gap, the IMDEA Materials team investigated the effects of long-term hygrothermal ageing by exposing PLA nanocomposites to conditions representative of real-world environments: 40°C and 75% relative humidity for six months.

Each of the composite materials contained one of three two-dimensional nanofillers: organomodified nanoclay (NC), graphene nanoplatelets (GNP) or hexagonal boron nitride (hBN). The objective was to determine how these nanomaterials influence the degradation behaviour of PLA during prolonged exposure to humidity.

After six months, moisture uptake remained between just 0.3% and 0.7% by weight, yet mechanical and rheological testing revealed deterioration in material performance.

Neat PLA, and PLA reinforced with NC, experienced severe losses in impact resistance, with impact strength decreasing by around 80%. Rheological analysis also revealed a dramatic reduction in melt viscosity, indicating extensive degradation of the polymer structure.

These results demonstrate that even limited exposure to moisture can have significant consequences for the long-term performance of biodegradable polymers.

Among all the nanomaterials investigated, hexagonal boron nitride (hBN) delivered the best overall performance.

The hBN-reinforced nanocomposite retained approximately 86% of its original impact toughness after six months of ageing, significantly outperforming the other formulations. Thermal analysis further showed that the filler helped maintain a stable crystallisation behaviour throughout the conditioning period.

The results also indicated that hBN helped preserve the rheological properties of PLA during ageing. Together, these findings suggest that hBN is a promising nanofiller for improving the performance of PLA-based materials under prolonged humid conditions.

Importantly, researchers distinguished between two often-confused yet separate phenomena: plasticisation and chemical degradation.

“We found that short-term exposure to liquid water primarily causes plasticisation, a reversible process in which absorbed water increases polymer chain mobility,” said Chovancová. “This effect can temporarily improve toughness and flexibility, even while initial degradation processes begin”.

“Long-term exposure to humidity, however, follows a different path”. “Over time, moisture promotes hydrolytic chain scission, progressively breaking down polymer chains within the material”. “This irreversible chemical degradation ultimately results in embrittlement, reduced toughness and a collapse in melt viscosity,” she concluded.

The findings provide new insights into the long-term behaviour of PLA nanocomposites and may help guide the development of biodegradable materials for applications where exposure to humidity is an important consideration.

The work presented here is a part of the PID2023-150813OB-I00 project funded by MICIU/AEI/10.13039/501100011033 and the EU’s FEDER funds.